WEI Zhi-Feng1,2, CHEN Xiao-Long1, CHE Guang-Can1, WANG Fu-Ming2, LI Wen-Chao2, HE Meng1
1Institute of Physics and Center for Condensed Matter Physics, Chinese Academy of Science, Beijing 100080
2Department of Physical Chemistry, University of Science and Technology Beijing, Beijing 100083
1Institute of Physics and Center for Condensed Matter Physics, Chinese Academy of Science, Beijing 100080
2Department of Physical Chemistry, University of Science and Technology Beijing, Beijing 100083
Abstract: We have determined the Debye temperature of the MgCNi3 superconductor by using the Rietveld refinement method based on the powder x-ray diffraction data. MgCNi3 crystallizes in the cubic perovskite structure with space group Pm3m and lattice constant a = 3.8089Å. The temperature factors of the atoms Mg, C and Ni are 0.52, 0.45 and 0.44, respectively. The Debye temperature of MgCNi3 is calculated to be D = 440K.
WEI Zhi-Feng;CHEN Xiao-Long;CHE Guang-Can;WANG Fu-Ming;LI Wen-Chao;HE Meng. Debye Temperature of the MgCNi3 Superconductor
[J]. 中国物理快报, 2002, 19(2): 249-251.
WEI Zhi-Feng, CHEN Xiao-Long, CHE Guang-Can, WANG Fu-Ming, LI Wen-Chao, HE Meng. Debye Temperature of the MgCNi3 Superconductor
. Chin. Phys. Lett., 2002, 19(2): 249-251.