Large Non-resonant Nonlinear Optical Susceptibility of Cu2 O Microcrystallites
WANG You-gui, SI Jin-hai, ZHAO Jiang, ZOU Bing-suo, YE Pei-xian
Institute of Physics, Chinese Academy of Sciences, Beijing 100080
Large Non-resonant Nonlinear Optical Susceptibility of Cu2 O Microcrystallites
WANG You-gui;SI Jin-hai;ZHAO Jiang;ZOU Bing-suo;YE Pei-xian
Institute of Physics, Chinese Academy of Sciences, Beijing 100080
关键词 :
42.65.An ,
42.70.Nq
Abstract : We report the measured results of non-resonant nonlinearity by degenerate four-wave mixing for Cu2 O nanoparticles having central diameter of 9nm. The value of (3) obtained in a 10ns pulse experiment is 8.48 x 10-10 esu, and the nonlinear response time of the sample is estimated to be in the order of nanosecond.
Key words :
42.65.An
42.70.Nq
出版日期: 1996-03-01
:
42.65.An
(Optical susceptibility, hyperpolarizability)
42.70.Nq
(Other nonlinear optical materials; photorefractive and semiconductor materials)
引用本文:
WANG You-gui;SI Jin-hai;ZHAO Jiang;ZOU Bing-suo;YE Pei-xian. Large Non-resonant Nonlinear Optical Susceptibility of Cu2 O Microcrystallites[J]. 中国物理快报, 1996, 13(3): 182-184.
WANG You-gui, SI Jin-hai, ZHAO Jiang, ZOU Bing-suo, YE Pei-xian. Large Non-resonant Nonlinear Optical Susceptibility of Cu2 O Microcrystallites. Chin. Phys. Lett., 1996, 13(3): 182-184.
链接本文:
https://cpl.iphy.ac.cn/CN/
或
https://cpl.iphy.ac.cn/CN/Y1996/V13/I3/182
[1]
WU Qiang;XU Jing-Jun;RUPP Romano;ZHANG Xin-Zheng;LOU Ci-Bo;BUGAYCHUK Sveta. Transition from Backscattering Speckles to Phase Conjugation in LiNbO3 :Fe [J]. 中国物理快报, 2006, 23(8): 2101-2104.
[2]
JIN Zhao-Hui;LI Zhong-Yu;KASATANI Kazuo;OKAMOTO Hiroaki. Anisotropy in Third-Order Nonlinear Optical Susceptibility of a Squarylium Dye in a Nematic Liquid Crystal [J]. 中国物理快报, 2006, 23(3): 635-638.
[3]
ZHU Rong-Yi;QIU Xue-Qiong;CHEN Yu;QIAN Shi-Xiong. Nonlinear Optical Properties of Indium Phthalocyanine Axially Grafted Polystyrene Thin Film [J]. 中国物理快报, 2006, 23(3): 622-624.
[4]
JIN Zhao-Hui;LI Zhong-Yu;KASATANI Kazuo;OKAMOTO Hiroaki. Fast Optical Switching Using Oriented Cyanine Dye-Doped Nematic Liquid Crystal [J]. 中国物理快报, 2006, 23(10): 2786-2789.
[5]
LI Guang-Ming;WAN Yu-Hong;JIANG Zhu-Qing;TAO Shi-Quan. Holographic and Thermal-Fixing Characteristics of Doubly Doped Zn:Fe:LiNbO3 Crystals [J]. 中国物理快报, 2006, 23(10): 2782-2785.
[6]
CHEN Dai-Jian;DING Sha;HAN Jun-Bo;ZHOU Hui-Jun;XIAO Si;XIONG Gui-Guang;WANG Qu-Quan;. A Sign Alternation of Nonlinear Absorption in Gold Composite Films in Z-Scan [J]. 中国物理快报, 2005, 22(9): 2286-2289.
[7]
LI Zhong-Yu;JIN Zhao-Hui;KASATANI Kazuo;OKAMOTO Hiroaki. Large Third-Order Optical Nonlinearity and Fast Response of a Squarylium Dye [J]. 中国物理快报, 2005, 22(9): 2282-2285.
[8]
ZHANG Xue-Ru;OUYANG Qiu-Yun;WANG Yu-Xiao;JIANG Li;SONG Ying-Lin;LI Yu-Liang;WEI Tai-Huei. Nonresonant Saturation Absorption in Electrostatic Self-Assembly Films Containing Methanofullerene [J]. 中国物理快报, 2005, 22(8): 1898-1901.
[9]
FU Gang;Kazuo Kasatani;Hiroaki Okamoto;Shunsuke Takenaka. Large and Fast Resonant Third-Order Optical Nonlinearities of Silicon 2,3-Naphthalocyanine Bi (trihexylsilyloxide) [J]. 中国物理快报, 2005, 22(7): 1687-1690.
[10]
DAI Cui-Xia;LIU Li-Ren;LIU De-An;CHAI Zhi-Fang. Sensitivity Improvement by UV-Light Recording in LiNbO3 :Ce:Cu Crystals [J]. 中国物理快报, 2005, 22(5): 1127-1130.
[11]
TANG Li-Qin;ZHAO Li-Juan;ZHANG Xin-Zheng;YU Hua;MENG Jie;LIANG Qin;XU Jing-Jun;KONG Yong-Fa. Luminescent Enhancement in Mg- and Er-Codoped LiNbO3 Crystals [J]. 中国物理快报, 2005, 22(3): 588-590.
[12]
ZHANG Chun-Feng;YOU Guan-Jun;DONG Zhi-Wei;LIU Ye;MA Guo-Hong;QIAN Shi-Xiong. Off-Resonant Third-Order Optical Nonlinearity of an Ag:TiO2 Composite Film [J]. 中国物理快报, 2005, 22(2): 475-477.
[13]
LI Guang-Bo;GONG Zhao;JIA Ke-Miao;LONG Wen-Hua;YANG Jian-Yi;JIANG Xiao-Qing;WANG Yue-Lin;WANG Ming-Hua. Compact Arrayed-Waveguide Grating on Silicon-on-Insulator with Integrated Waveguide Turning Mirrors [J]. 中国物理快报, 2005, 22(12): 3100-3103.
[14]
FENG Lin;WANG Yan-Ling;REN Quan;ZHGNG Guang-Hui;YANG Hong-Liang;SUN Xiang-Bing. Third-Order Optical Nonlinearity of a Novel Material: (Tetramethylammonium)bis(1,3-dithiole-2-thione-4,5-dithiolato) Copper [J]. 中国物理快报, 2005, 22(11): 2834-2836.
[15]
WANG Zhen-Hua;ZHANG Xin-Zheng;XU Jing-Jun;WU Qiang;QIAO Hai-Jun;TANG Bai-Quan;RUPP Romano;KONG Yong-Fa;CHEN Shao-Lin;HUANG Zi-Heng;LI Bing;LIU Shi-Guo;ZHANG Ling. Time-Resolved Femtosecond Degenerate Four-Wave Mixing in LiNbO3 :Fe,Mg Crystal [J]. 中国物理快报, 2005, 22(11): 2831-2833.